4mm 5mm 6mm 8mm 10mm 12mm 15mm 19mm Tempered Glass Heat Soaked

4mm 5mm 6mm 8mm 10mm 12mm 15mm 19mm Tempered Glass Heat Soaked
4mm 5mm 6mm 8mm 10mm 12mm 15mm 19mm Tempered Glass Heat Soaked4mm 5mm 6mm 8mm 10mm 12mm 15mm 19mm Tempered Glass Heat Soaked4mm 5mm 6mm 8mm 10mm 12mm 15mm 19mm Tempered Glass Heat Soaked4mm 5mm 6mm 8mm 10mm 12mm 15mm 19mm Tempered Glass Heat Soaked
group name
Flat Tempered Glass
Min Order
20 square meter
brand name
AoHong
model
Tempered Glass Heat Soaked
Nearest port for product export
XinGang Tianjin, Dalian, QingDao
Delivery clauses under the trade mode
FOB, CFR, CIF, EXW, FAS, CIP, FCA, CPT, DEQ, DDP, DDU, Express Delivery, DAF, DES
Acceptable payment methods
T/T, L/C, Credit Card, PayPal, Westem Union, Cash, Escrow
update time
Mon, 15 Oct 2018 17:16:40 GMT

Paramtents

  • Type Tempered Glass Heat Soaked

  • Availble Color Clear ,green,blue,grey ,pink, bronz

  • Availble Thickness 4mm 5mm 6mm 8mm 10mm 12mm 15mm 19mm

  • Certificate ISO BV CE CCC

  • Application window,door,table top,furniture,show room,etc

  • Mix size 100mm*100mm

  • Max size 3000mm*7000mm

  • Test Broken >40pcs per m2

  • Size Tolerance +/- 1.0mm

  • Hole Tolerance +/- 1.0mm

Packging & Delivery

  • Min Order20 square meter

Briefing

Heat soaking is a process that may expose NiS inclusions in tempered glass thereby reducing risk of potential field cracking.

Detailed

Tempered Glass Heat Soaked 

All float glass contains some level of imperfection. One type of imperfection is nickel sulfide (NiS) inclusion. Most NiS inclusions are stable and cause no problems. There is, however, the potential for NiS inclusions that may cause spontaneous breakage in tempered glass without any load or thermal stress being applied.

Heat soaking is a process that may expose NiS inclusions in tempered glass thereby reducing the risk of potential field cracking. The process involves placing the tempered glass inside a chamber and raising the temperature to approximately 290ºC to accelerate nickel sulfide expansion. This causes glass containing nickel sulfide inclusions to break in the heat soak chamber.